What is the minimum distance that a nozzle can be to the seam which joins a shell and a F&D head?
 
Replies continue below

Recommended for you

boy that's a loaded question

fully depends on a number of things.

per code, your nozzle can be slap dab in the middle of the seam if you follow it's rules for nde/radiograpy and have designed for it.

in the real world, it is best to have it one nominal nozzle size between the center of seam and center of nozzle so there are no problems with reinforcement overlap.

as a minimum for exempt nozzles, I like the welds to clear each other by at least an inch.

but if physical limitations exist, you can have the nozzle in the seam
 
Thanks for the clear response...
 
This does depend on which code is being used. For example, EN 13445 does have some limitations regarding nozzles to seams and structural discontinuties (cone to cylinder junctions for example)
 