Jun 24, 2016 #1 Macdost Materials Joined Nov 20, 2014 Messages 30 Location CA I have a database with NA equivalents to Euro grades, the following I cannot find, anyone have equivalents?: 10CrMOVNb9 22CrMoV12 21CrMoNiV4 I appreciate any assistance on this, thank you
I have a database with NA equivalents to Euro grades, the following I cannot find, anyone have equivalents?: 10CrMOVNb9 22CrMoV12 21CrMoNiV4 I appreciate any assistance on this, thank you
Jun 24, 2016 #2 EdStainless Materials Joined May 20, 2004 Messages 16,373 Location Waukesha WI USA My 2013 Stahlschlussel does not list any of these grades. What specs are they listed in? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
My 2013 Stahlschlussel does not list any of these grades. What specs are they listed in? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Jun 24, 2016 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US These look like power generation steels for turbine parts; http://www.vallourec.com/fossilpower/EN/Products/Pages/tp91.aspx SA 213 T91 is close 22CrMoV12 Looks like a martensitic stainless steel with V 21CrMoNiV4 This looks like a 1 Cr-0.7Mo- 1Ni - 0.25V turbine rotor steel Upvote 0 Downvote
These look like power generation steels for turbine parts; http://www.vallourec.com/fossilpower/EN/Products/Pages/tp91.aspx SA 213 T91 is close 22CrMoV12 Looks like a martensitic stainless steel with V 21CrMoNiV4 This looks like a 1 Cr-0.7Mo- 1Ni - 0.25V turbine rotor steel