Hello all,
I have a problem with defining nonlinearity to a material. first i have defined
MP, EX, 1, 206000e6
MP, PRXY, 1, 0.3
MP, DENS, 1, 7850
for steel, and then i input and
TB,KINH,1,1,8 ! Activate a data table
TBTEMP,
TBPT,,0.00 , 0.0 ! Strain = 0.00, Stress = 0.000
TBPT,,0.0029 , 320.7e6 ! Strain = 0.0029, Stress = 320.7
TBPT,,0.0092 , 350.6e6
TBPT,,0.0356 , 381.9e6
TBPT,,0.1006 , 411.9e6
TBPT,,0.2056 , 426.1e6
TBPT,,0.2518 , 420.2e6
TBPT,,0.2812 , 387.0e6
TBPT,,0.2975 , 331.6e6
when i start the solution it comes with this error:
*** ERROR *** CP = 23.516 TIME= 16:21:25
For material 1 at temperature 0, the initial slope of the stress-strain
curve based on the TB,KINH table ( 1.105862069E+11 ) is less than EX (
2.06E+11 ).
I tried not to define the EX, and the it says that EX is not defined...
If anyone have an idea how can i fix this i'll be very grateful.
Thanks
I have a problem with defining nonlinearity to a material. first i have defined
MP, EX, 1, 206000e6
MP, PRXY, 1, 0.3
MP, DENS, 1, 7850
for steel, and then i input and
TB,KINH,1,1,8 ! Activate a data table
TBTEMP,
TBPT,,0.00 , 0.0 ! Strain = 0.00, Stress = 0.000
TBPT,,0.0029 , 320.7e6 ! Strain = 0.0029, Stress = 320.7
TBPT,,0.0092 , 350.6e6
TBPT,,0.0356 , 381.9e6
TBPT,,0.1006 , 411.9e6
TBPT,,0.2056 , 426.1e6
TBPT,,0.2518 , 420.2e6
TBPT,,0.2812 , 387.0e6
TBPT,,0.2975 , 331.6e6
when i start the solution it comes with this error:
*** ERROR *** CP = 23.516 TIME= 16:21:25
For material 1 at temperature 0, the initial slope of the stress-strain
curve based on the TB,KINH table ( 1.105862069E+11 ) is less than EX (
2.06E+11 ).
I tried not to define the EX, and the it says that EX is not defined...
If anyone have an idea how can i fix this i'll be very grateful.