P
pjw
Guest
My question is, is there any way to apply non-linear shrinkage allownance to a prt. For example if you had an equation relating shrinkage to distance from a co-ordinate system? My problem is that thin sections and thick sections of castings we produce don't always shrink in a linear fashion and when it comes to producing the dies, the models we use to cut-out the cavities in the models have to be representitive of the finished prduct plus the shrinkage.