Hello,
I am working on a non-linear contact problem in Ansys Apdl. In the material models i am trying to input strain and stress values for the multilinear plasticity. In the project description we were given several points ploted on a graph of "engineering stress and strain". The 0.2% yield stress has a value of 735 MPa and the young's modulus 200GPa. Now if I want to put the points of "stress Vs plastic strain" should i convert the "engineering stress and strain" points from the graph given to "true stress and strain"? If that's so then here are my calculations for one point.
The next "engineering stress" point provided after the yield stress is 738Mpa and the equivalent strain point is 0.848%
i know that eps(true)=ln(1+eps(eng))
and that Sigma(true)=Sigma(eng)*(1+eps(eng))
therefore eps(true)=ln(1+0.848)=0.614%
and Sigma(true)=738*(1+0.00848)=744.26MPa
The true eps(elastic)=Sigma(true)/E=744.25/200000=0.00372
The true eps(plastic)=eps(true)-eps(elastic)=0.00614-0.00372=0.00242 or 0.242%
Is my thinking correct?
Thank you in advance
I am working on a non-linear contact problem in Ansys Apdl. In the material models i am trying to input strain and stress values for the multilinear plasticity. In the project description we were given several points ploted on a graph of "engineering stress and strain". The 0.2% yield stress has a value of 735 MPa and the young's modulus 200GPa. Now if I want to put the points of "stress Vs plastic strain" should i convert the "engineering stress and strain" points from the graph given to "true stress and strain"? If that's so then here are my calculations for one point.
The next "engineering stress" point provided after the yield stress is 738Mpa and the equivalent strain point is 0.848%
i know that eps(true)=ln(1+eps(eng))
and that Sigma(true)=Sigma(eng)*(1+eps(eng))
therefore eps(true)=ln(1+0.848)=0.614%
and Sigma(true)=738*(1+0.00848)=744.26MPa
The true eps(elastic)=Sigma(true)/E=744.25/200000=0.00372
The true eps(plastic)=eps(true)-eps(elastic)=0.00614-0.00372=0.00242 or 0.242%
Is my thinking correct?
Thank you in advance