Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

non-hexavalent chrome coatings 1

Status
Not open for further replies.

67bonnie

Mechanical
Jul 31, 2007
6
does anyone know where i can find a ranking of the costs of the non- hexavalent chrome coatings that are used for fasteners. I found this very helpful posting with a table of the coatings ranked by corrosion resistance, but not cost. thread332-189454. can I assume that the least effective are the cheapest?
 
Replies continue below

Recommended for you

Yes, you can assume that the least effective are the least expensive.

The lowest performance on that chart is a simple zinc phosphate, with a relative cost of 1.

DELTATONE / DORRELTECH B17 14 µ would have a relative cost of 6.

Geomet is 7.

Zinc platings with TRIVALENT chromate conversion coatings have relative cost > 10.

So, the high-performing zinc-flake coatings are less expensive than the lower-performing zinc platings. Food for thought.