Hi everyone, i'd like to specify node temperature in static/general analysis. Im trying to do this by using predefined field, but it doesn't work. I read in Abaqus user manual that I should use input file options, where inputed file contains node number, temperature value. Could anyone tell me what am I doing wrong? Here is my INP file:
*Heading
** Job name: kostka Model name: Model-1
** Generated by: Abaqus/CAE 6.10-1
*Preprint, echo=NO, model=NO, history=NO, contact=NO
**
** PARTS
**
*Part, name=Part-1
*Node
1, -25., -25., 50.
2, -25., 0., 50.
3, -25., 25., 50.
4, -25., -25., 25.
5, -25., 0., 25.
6, -25., 25., 25.
7, -25., -25., 0.
8, -25., 0., 0.
9, -25., 25., 0.
10, 0., -25., 50.
11, 0., 0., 50.
12, 0., 25., 50.
13, 0., -25., 25.
14, 0., 0., 25.
15, 0., 25., 25.
16, 0., -25., 0.
17, 0., 0., 0.
18, 0., 25., 0.
19, 25., -25., 50.
20, 25., 0., 50.
21, 25., 25., 50.
22, 25., -25., 25.
23, 25., 0., 25.
24, 25., 25., 25.
25, 25., -25., 0.
26, 25., 0., 0.
27, 25., 25., 0.
*Element, type=C3D8R
1, 10, 11, 14, 13, 1, 2, 5, 4
2, 11, 12, 15, 14, 2, 3, 6, 5
3, 13, 14, 17, 16, 4, 5, 8, 7
4, 14, 15, 18, 17, 5, 6, 9, 8
5, 19, 20, 23, 22, 10, 11, 14, 13
6, 20, 21, 24, 23, 11, 12, 15, 14
7, 22, 23, 26, 25, 13, 14, 17, 16
8, 23, 24, 27, 26, 14, 15, 18, 17
*Nset, nset=_PickedSet2, internal, generate
1, 27, 1
*Elset, elset=_PickedSet2, internal, generate
1, 8, 1
** Section: Section-1
*Solid Section, elset=_PickedSet2, material=Cu_mm
,
*End Part
**
**
** ASSEMBLY
**
*Assembly, name=Assembly
**
*Instance, name=Part-1-1, part=Part-1
*End Instance
**
*Nset, nset=_PickedSet15, internal, instance=Part-1-1, generate
1, 27, 1
*Elset, elset=_PickedSet15, internal, instance=Part-1-1, generate
1, 8, 1
*End Assembly
*Amplitude, name=Amp-1
0., 0., 1., 1.
**
** MATERIALS
**
*Material, name=Cu_mm
*Conductivity
0.39,
*Density
8.9e-06,
*Elastic
110000., 0.37
*Expansion
2.4e-05,
*Plastic
45., 0.
225., 0.5
*Specific Heat
390.,
** ----------------------------------------------------------------
**
** STEP: Step-1
**
*Step, name=Step-1
*Static
1., 1., 1e-05, 1.
**
** PREDEFINED FIELDS
**
** Name: Predefined Field-1 Type: Temperature
*INCLUDE, INPUT=job-4.inp
**
** OUTPUT REQUESTS
**
*Restart, write, frequency=0
**
** FIELD OUTPUT: F-Output-1
**
*Output, field
*node output
CF, NT, RF, U
*Output, field, variable=PRESELECT
**
** HISTORY OUTPUT: H-Output-1
**
*Output, history
*Contact Output
SJD, SJDA, SJDT, SJDTA
*End Step

where node-temp.inp is:
1, 10
...
...
...
27, 100

Abaqus accept this input file syntax, but after analysis all node temp value are 0. I read in chapter about input file syntax rules that there should be *KEYWORD followed by data lines.
*TEMPERATURE
1, 10
...
...
...
27, 100

But when i add keyword *TEMPERATURE to my input file analysis doesn't work, there is an error "Error in Job-1, in keyword *TEMPERATURE, file "node-temp.inp", Unknown assembly id1.


Thanks for any help

 
Replies continue below

Recommended for you

Hey!I'm facing the same problem..Please share if you managed to sort it out!


All help deeply appreciated,

Ankit
 
Hi Stancler,

Have you figured out your problem? I have a similar problem, if you can give me some information, it'll be very helpful.
 
My suggestion is to apply the individual temperatures on each node in CAE
 
In general ABAQUS refers to a node, element or set in an instance by specifying name-of-assemble.name-of-instance.ID-of object
 
Correction to my previous post:

In the file node-temp.inp, you need to have definitions as follows:

Part-1-1.1, 10 instead of 1, 10
..
..
Part-1-1.27, 100 instead of 27, 100

Why? Because Part-1-1 is the name of the instance of the part (Part-1) that you created. Another option is to have a flat input deck and then, 1 will work just as well.