I need to approve a WPS for UNS S20910 Hot Rolled Material (also named Nitronic 50/XM-19). I found maximum hardness values in the base material zone up to 363 HV.
NACE said "However, S20910 is acceptable in the annealed or hot-rolled (hot/cold-worked) condition at a maximum hardness of 35 HRC"
NACE also said "Individual HRC readings exceeding the value
permitted by this part of ISO 15156 may be considered acceptable if the average of several readings taken
within close proximity does not exceed the value permitted by this part of ISO 15156 and no individual reading
is greater than 2 HRC above the specified value"
37 HRC corrospond exactly to 363 HV10, but my problem is that 5 hardness point exceed 35 HRC.
Is this WPS technically acceptable or we need to requalified the procedure.
NACE said "However, S20910 is acceptable in the annealed or hot-rolled (hot/cold-worked) condition at a maximum hardness of 35 HRC"
NACE also said "Individual HRC readings exceeding the value
permitted by this part of ISO 15156 may be considered acceptable if the average of several readings taken
within close proximity does not exceed the value permitted by this part of ISO 15156 and no individual reading
is greater than 2 HRC above the specified value"
37 HRC corrospond exactly to 363 HV10, but my problem is that 5 hardness point exceed 35 HRC.
Is this WPS technically acceptable or we need to requalified the procedure.