suthagarqa
Petroleum
Hi Team,
Recently we weld with Nicr-A on N06625 using GTAW but at the end of welding, we found cracks.
So, we grind the crack area & re-weld. But, Crack become worse.
Need before & after weld guide and advise to avoid crack.
Thanks.
Recently we weld with Nicr-A on N06625 using GTAW but at the end of welding, we found cracks.
So, we grind the crack area & re-weld. But, Crack become worse.
Need before & after weld guide and advise to avoid crack.