May 14, 2004 #1 limct Mechanical Joined Jan 27, 2003 Messages 134 Location HK Anyone know about the detail of the following nickels? Nickel 201 CR 1/2H (half hard??) Nickel 201 CR 1/2K (???) Appreciate your valuable advise. Best regards, ct
Anyone know about the detail of the following nickels? Nickel 201 CR 1/2H (half hard??) Nickel 201 CR 1/2K (???) Appreciate your valuable advise. Best regards, ct
May 14, 2004 1 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Nickel alloy 201 is essentially pure nickel. You can obtain more information about composition and properties from Special Metals, the leading producer of nickel-based alloys: http://www.specialmetals.com/documents/Nickel 200 & 201.pdf Upvote 0 Downvote
Nickel alloy 201 is essentially pure nickel. You can obtain more information about composition and properties from Special Metals, the leading producer of nickel-based alloys: http://www.specialmetals.com/documents/Nickel 200 & 201.pdf