New AISC Publication Article 1

Status
Not open for further replies.
Sometimes, I feel kind of dumb when I read an article like that. Just some good rules of thumb for deciding what type of weld to use. Stuff that I rarely think about, but really should be more "intentional" about in design!
 
Concur...

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
Never miss a chance of reading anything by Duane Miller!
 
He's great...

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
What's the trick with Figure 4a vs 4b? He says 22% difference in weight of weld metal but the difference in area is 80%. Does it have to do with building out at the edges, or melting away the base metal?

And Fig 1b has slightly less capacity than 1a?
 