Neoprene Lifetime

Status
Not open for further replies.

pairoch

Mechanical
May 5, 2002
2
Dear sir,
Can anyone give us some information regarding Neoprene Rubber lifetime??
 
Replies continue below

Recommended for you

Dear Sir
ref your question neoprene life is one year in 25c
1329
 