Hi people.
Plase look at the sketch attached.
Short description:
Virgin ground under the future raft slab is removed (aboth 20cm).
Beam trenches are dig out.
Beams are poured first and serve later as the "side formwork" for good hardcore compaction.
Virgin ground (slab part) is compacted and then filled with harcore compacted filling (fractions raging from 1-32mm).
An "mud slab" is poured (above the harcore fill) wich then serves as the leveling plane for the proper reinforecement placement.
Beams are poured first and later serev as the "side formwork" for good hardcore compaction.
Hidroisolation is placed on the raft surface as the first layer of the residential floor.
note: virgin ground level (left in green) and the down side of the RC raft slab are at the same elevation.
Im interested in your negative comments for this design.
Thank you.
Plase look at the sketch attached.
Short description:
Virgin ground under the future raft slab is removed (aboth 20cm).
Beam trenches are dig out.
Beams are poured first and serve later as the "side formwork" for good hardcore compaction.
Virgin ground (slab part) is compacted and then filled with harcore compacted filling (fractions raging from 1-32mm).
An "mud slab" is poured (above the harcore fill) wich then serves as the leveling plane for the proper reinforecement placement.
Beams are poured first and later serev as the "side formwork" for good hardcore compaction.
Hidroisolation is placed on the raft surface as the first layer of the residential floor.
note: virgin ground level (left in green) and the down side of the RC raft slab are at the same elevation.
Im interested in your negative comments for this design.