I need to x-ray & /or Ultrasonic test some parts made from Carburized AISI 9310 steel, 3 of 5 parts had heat treat cracks.
I need to verify the two parts do not have cracks below sub-surface. any recommendations?
parts past mag particle insp,but I want to make sure there are no defects at the center.
Thanks
Mfgenggear
I need to verify the two parts do not have cracks below sub-surface. any recommendations?
parts past mag particle insp,but I want to make sure there are no defects at the center.