Hello everyone,
We are working with 4130 for a part we are building and need to reach a Charpy impact result of at least 25 ft-lbs (avg.). We are falling way short (we are at 10, 4, 5...). From what I understand, results have been improved in the past by heat treating. Heat treating seems like it would hurt more than help in this case. What can I do to improve the results for the 4130?
Also, our tensile results are ~48,000 psi for yield, 87,000 psi ultimate; both seem low. But, our elongation at break is around 18% or so, which seems high...
I wish I had more data to give, but that is all I have at this point. Any suggestions?
Thanks
We are working with 4130 for a part we are building and need to reach a Charpy impact result of at least 25 ft-lbs (avg.). We are falling way short (we are at 10, 4, 5...). From what I understand, results have been improved in the past by heat treating. Heat treating seems like it would hurt more than help in this case. What can I do to improve the results for the 4130?
Also, our tensile results are ~48,000 psi for yield, 87,000 psi ultimate; both seem low. But, our elongation at break is around 18% or so, which seems high...
I wish I had more data to give, but that is all I have at this point. Any suggestions?
Thanks