dculp1

Mechanical
May 16, 2006
75
I need a small quantity (~ 1 m) of Ti-6Al-4V seamless tubing. The size would be near 1" schedule 40 (1.315" OD x 1.049" ID); the size could be somewhat smaller or larger.

I found a company that could supply this in Grade 2 but not Ti-6Al-4V. Any suggestions?

Thanks,
Don Culp
 
Replies continue below

Recommended for you

aircraft hydraulic lines are cold finished seamless 6-4. It is in a high strength condition and much lighter wall that you want, but it is common.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Here is what EdStainless was referring to. You can get up to 1/2 the wall thickness of titanium pipe. If you find any one that carries anything close to your requirements make sure you give them a call.


The reason that the CP grades are readily available is that they are used in the chemical process industry were 6-4 is mainly a structural material where weight saving are important.
 
Unclesyd --

Despite their web sites, Alloy Metals and Snappy Metals no longer handle Ti tubing or pipe. Any other suggestions?

Thanks,
Don Culp
 
EdStainless: out of curiosity, how are these hydraulic lines connected? I've never been close enough to aircraft to notice...
 
They orbital weld end fittings and have captive nuts. I believe that Allen Aircraft makes a lot of the fittings. We make the exact same size and strength tubing in stainless 21-6-9. It has the same pressure rating but it is used in locations that might be subject to damage. The 21-6-9 has much greater damage resistance. The SS doesn't use welded ends but a special collar system.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 