We are trying to come up with a solution to a bushing problem. We have a bushing in an reversing application where a sleeve rotates +/- 15° within a bushing continuously. The sleeve has a 2-3/4" OD for reference.
I need something that will withstand a Velocity of V=210 fpm, P= 2000 psi (force that pin puts on projected area of bushing), and a pv value around 450,000.
An initial attempt was Mag-bronze with grease. After running through these numbers I can see why it didn't work.
Mag Bronze Max P=8,000 , Max V = 100, max PV=150,000
Any ideas?
Thanks,
Schroyer
I need something that will withstand a Velocity of V=210 fpm, P= 2000 psi (force that pin puts on projected area of bushing), and a pv value around 450,000.
An initial attempt was Mag-bronze with grease. After running through these numbers I can see why it didn't work.
Mag Bronze Max P=8,000 , Max V = 100, max PV=150,000
Any ideas?
Thanks,
Schroyer