I'm looking for a material that will be able to withstand very high temperatures (>1200 C) for periods of about 2 minutes.
The material is needed as a heat shield for a stainless steel fume hood that collects the fume created by pouring molten steel into a furnace. Because it will be in a fume hood, the material must also be immune to chemical attack.
We currently use 3/4" cast iron plates, but they are being melted and/or corroded away.
Price is a consideration since the area to be covered is quite large (approximately 125 square feet)
I'd appreciate any suggestions.
The material is needed as a heat shield for a stainless steel fume hood that collects the fume created by pouring molten steel into a furnace. Because it will be in a fume hood, the material must also be immune to chemical attack.
We currently use 3/4" cast iron plates, but they are being melted and/or corroded away.
Price is a consideration since the area to be covered is quite large (approximately 125 square feet)
I'd appreciate any suggestions.