Hi,
What’s cutting condition to cut 1/4” thick mild steel on Mitsubishi LVP 3015 40 CFX? Thanks.
 
Thanks laserkatana. Can I cut this material using nitrogen?
 
You can try using a B01 nozzle and if there is a supplied cut condition for .250" MS with N2, if not use a SS Conditions of equivalent thickness.
 
There are many ways to cut mild steel plate, some of which are suited for automation some are not. Some are suited for thinner plate, some for thicker. Some are fast, some are slow. Some are low-cost, some expensive.
 