VipulAkabari
Mechanical
Hi Friends..
Hope all have a nice day..
I have Amada 3015NT 4KW Laser machine, I try to cut 3 mm thick Aluminium with air, but i found some hard burrs and some time it reflect.
Please suggest me for reduce burrs..
Hope all have a nice day..
I have Amada 3015NT 4KW Laser machine, I try to cut 3 mm thick Aluminium with air, but i found some hard burrs and some time it reflect.
Please suggest me for reduce burrs..