Hi the machine is Amada Fo3015NT. we are not able to get a nice cut. Someone have cutting condition for this type of material?
 
Replies continue below

Recommended for you

try using the cut condition for stainless steel of the same thickness, but change your assist gas to shop air.
 
Thanks for your reply. I think we don't have a good air, cause we still have a lot of dross. not able to get a clean cut.
 
if you can post a picture of the parts edge and of the cut condition screen, there are a few really good experts here who can help a lot if you provide enough information. I am not an expert, but things i would try is lowering air pressure, going up and down with focus, increasing and decreasing feedrate.