Anybody know a good consulting place in China to tell me what american resins I would need to match a blown PE [LLDPE] film???
 
Replies continue below

Recommended for you

Have you tried local universities.

Have you tried mailing samples to off shore universities.

Have you asked PE resin suppliers to test it for you.

Are you sure it is single layer.

If it is single layer, a simple density test and melting point test and MFI test should reveal all. These are very simple tests with very simple equipment.

If it is multilayer, you will need to test each layer. That will require fancy microscopes and equipment for measuring crystallinity.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor