NDT of S.S Elbow 1

Status
Not open for further replies.

0481

Materials
Jul 2, 2007
15
I want to perform Ultrasonic testing of SS elbow od Dia:24 Inch with thickness of 30mm. Do any one know about procedure please let me know
 
Replies continue below

Recommended for you

Hire an ASNT qualified nondestructive testing (NDT) firm for this activity. They will have the procedure, calibration standard, and ASNT qualified UT examiners.
 
The big thing to watch out for with stainless steel is the use of calibration blcosk without welds (not specifically required by some specifications). Shear waves will work fine on the un-welded calibration block but will significantly under-test the weld. This can be readily seen if a welded block is used. All angle beam scans should be done with angle longitudinal waves.

Not all inspection houses have figured this out. Unfortunately, it is not obvious based on the screen display that the weld is being significantly under-tested.

JR97 (ASNT UT Level III)
 