What non-destructive test should I do on the self flange with 350-lf2 material?
 
Replies continue below

Recommended for you

Are you asking what is required by a code? If so, what code? Or, are you asking about general good industry practice?

Please provide some details of what you're working on - pressure / temperature / size / etc...
 
Dimensional, visual, liquid penetrant,.......
See SA-961