Sep 10, 2020 #1 azadfar Industrial Joined Jan 15, 2015 Messages 7 Location IR Hello all What non-destructive test should I do on the self flange with 350-lf2 material?
Sep 10, 2020 #2 marty007 Mechanical Joined Mar 8, 2012 Messages 622 Location CA Are you asking what is required by a code? If so, what code? Or, are you asking about general good industry practice? Please provide some details of what you're working on - pressure / temperature / size / etc... Upvote 0 Downvote
Are you asking what is required by a code? If so, what code? Or, are you asking about general good industry practice? Please provide some details of what you're working on - pressure / temperature / size / etc...
Sep 10, 2020 #3 r6155 Mechanical Joined Jan 12, 2010 Messages 3,013 Location AR Dimensional, visual, liquid penetrant,....... See SA-961 Regards Upvote 0 Downvote