EngMan40
Civil/Environmental
- Jan 11, 2009
- 66
Base metals: 10" thick A36 bearing Plate with 6" A36 plate (part of box column). weld size 1/2" done using SMAW with E7018. 225F preheat was applied but only 3" depth into the metal not the the whole 10" from point of welding. Also was not maintained during welding. I want to check the whole weld not just the surface. any suggestions/ NDE method work best.