We usually use SA-106B seamless pipe, but due to size and availability issues are now contemplating the use of API 6L GrB PSL1.

I have the chemical, mechanical, and hydrotest specs, but haven't been able to find the welding NDE specs of the pipe. Does anyone have a quick reference or know of what NDE is used?

John
Mechanical Engineer
Artisan Industries Inc.
 
Replies continue below

Recommended for you

Essentially API 5L requires the long seam be 100% inspected either by RT, UT or electromagnetic, depending on the joining method, eg ERW or SAW.

Note PSL 2 is a superior product
 