Looking for some opinions on National Standard Mig Welding Wire ER70S-3. Would like to hear from some people that have or are using the wire. Salesmen need not answer, I have one already.
 
Over the years we have used tons of NS wire. We have never used their large packages.

I can recall no problems with any of their products. It is product that was just used that people never paid any attention to since it caused no problems.
 