Hey everyone,
I am honored to join you here.
I am a materials engineer, I had project having 3 phase separator projects in GOSP, so this separator is totally cladded from as per my selection based on the severity of sour medium based on NACE 8x194 category evaluation.
So based on API SP 21534, for completely weld overlayed vessel HIC requirements are not required for the backing CS and SSC mitigation requirements (from my understanding only) is not mandated as well.
So my selection was CS without any additional requirements+SS316 weld overlay (NACE MR0175 compliance as per part 3)
My question here shall I consider NACE requirements as well for the backing carbon steel or as long as the vessel is completely cladded by weld overlay no need for nace compliance for CS
I am honored to join you here.
I am a materials engineer, I had project having 3 phase separator projects in GOSP, so this separator is totally cladded from as per my selection based on the severity of sour medium based on NACE 8x194 category evaluation.
So based on API SP 21534, for completely weld overlayed vessel HIC requirements are not required for the backing CS and SSC mitigation requirements (from my understanding only) is not mandated as well.
So my selection was CS without any additional requirements+SS316 weld overlay (NACE MR0175 compliance as per part 3)
My question here shall I consider NACE requirements as well for the backing carbon steel or as long as the vessel is completely cladded by weld overlay no need for nace compliance for CS