Table 1 of NACE MR 0175/ISO 15156-3 indicates allowable exceptions for items that are subjected to pressure less than 65 PSI (Absolute Pressure): Flow Lines, Gathering lines, field facilities etc.
Valve Stem and Trim: these are considered non pressure parts as per various definitions of API/ANSI.
1) Does that mean valve trimes are emempt from the requirement, That is, can ,A 479 (With out Sol Anneal)be used?
2) Also some of the tables (Like ATable 28) specifically address valve components for some material, whilst table A 1 (Inidicates exclusions against austenitic). When the Table 1 gives exception based on absolute pressure, why the table A 28 still includes non pressure components, is it not contradictory?
Valve Stem and Trim: these are considered non pressure parts as per various definitions of API/ANSI.
1) Does that mean valve trimes are emempt from the requirement, That is, can ,A 479 (With out Sol Anneal)be used?
2) Also some of the tables (Like ATable 28) specifically address valve components for some material, whilst table A 1 (Inidicates exclusions against austenitic). When the Table 1 gives exception based on absolute pressure, why the table A 28 still includes non pressure components, is it not contradictory?