Hi all,

I am looking for a long time for the best suited material model for POM polymer.
Currently the only test data I have is uniaxial stress strain curves in various strain rates, and I am building multi-linear isotropic material with the data I have and I am using different data (i.e measured in different strain rates) for different analysis that simulates different strain rates in real life.
I was reading about viscoelastic and viscoplastic material models and didnt quite understood what test data should I have and how to use these models in ANSYS structural.
My first question is : does my current method (multi linear with different curves for different strain rates) seems logical to you?
Second question : I was looking for some guide/manual/training material in the ANSYS portal on viscoelastic and viscoplastic modeling and couldnt find anything usefull, can some one send me to the right direction on this?

Thanks.
 
Hello,
Regarding your second question, you can find in the Ansys portal the training on viscoelastic and viscoplastic modelling by searching "nonlinear materials".
 