I have a limited conversion table for Chrysler steel specs that doesn't include MS 573. Can anyone tell me the SAE equivalent?
 
Replies continue below

Recommended for you

MS-573 has the following title: CARBON STEEL - AISI 1010, 1212, 1213M, 1215 OR 12L14. It then states "SEE MS-BAR". MS-BAR has the following description for MS-573:

Cold Formed parts shall be fabricated from MS-420 Steel (SAE 1010). Parts machined from bar stock may use these optional materials MS-200 (SAE 1212) and MS-420 (SAE 1010), MS-760 (SAE 1213 or 1215) and MS-3395 (SAE 12L14).
 