I have received NDE Report (Magnetic Particle Inspection) for wellhead material AISI 410. As per my knowledge AISI 410 is martensitic stainless steel having paramagnetic properties. Please let know wheather 410 is paramagnetic or ferromagnetic and applicability of MPI on it.

Regards
 
Hi gafoorkti

Look at this :

" Martensitic and Precipitation Hardenable Stainless Steels

All Martensitic and most precipitation Hardenable stainless steels are ferromagnetic. Due to the stresses induced by the hardening transformation, these grades exhibit permanent magnetic properties if magnetized in the hardened condition. For a given grade, the coercive force, Hc, tends to increase with increasing hardening, rendering these alloys more difficult to demagnetize.

Examples of martensitic stainless steels are Type 410, 416, 420, 440B and 17-4. "

Source : Magnetic Behavior of Stainless Steels
 
MPI is a very suitable surface nondestructive test (NDT) for martensitic stainless steels, like 403 or 410.
 