Dec 30, 2003 #1 erbi Automotive Joined Jan 13, 2003 Messages 4 Location NL Can somebody help me building a machine which increase the magnetic field of motor and can somebody tell what I need to have to measure the field ?
Can somebody help me building a machine which increase the magnetic field of motor and can somebody tell what I need to have to measure the field ?
Jan 2, 2004 #2 UKpete Electrical Joined Jan 6, 2002 Messages 463 Location GB If you mean to remagnetize the magnets this can be very difficult, depending on the type of magnet and their size. Magnetic field measurement is usually achieved using a gaussmeter (these have a Hall probe sensor): http://www.sypris.com/stm/content.asp?page_id=266http://www.hirst-magnetics.com/http://www.redcliffe.org.uk/index.php?id=38http://www.walkerscientific.com/Pro...gnetic_Measuring/Gaussmeters/gaussmeters.html Upvote 0 Downvote
If you mean to remagnetize the magnets this can be very difficult, depending on the type of magnet and their size. Magnetic field measurement is usually achieved using a gaussmeter (these have a Hall probe sensor): http://www.sypris.com/stm/content.asp?page_id=266http://www.hirst-magnetics.com/http://www.redcliffe.org.uk/index.php?id=38http://www.walkerscientific.com/Pro...gnetic_Measuring/Gaussmeters/gaussmeters.html
Feb 17, 2004 #3 jmurphy115 Automotive Joined Feb 17, 2004 Messages 2 Location US If you need more magnetic field, you can switch to RareEarth magnets instead of Ferrites. They are 3-4 times stronger than Ferritte magnets. For samples, contact companies like Dexter Magnetics or Magnet Sales. To measure magnets, http://www.magsys.de. They have inexpensive handheld gaussmeter. Upvote 0 Downvote
If you need more magnetic field, you can switch to RareEarth magnets instead of Ferrites. They are 3-4 times stronger than Ferritte magnets. For samples, contact companies like Dexter Magnetics or Magnet Sales. To measure magnets, http://www.magsys.de. They have inexpensive handheld gaussmeter.