aroundhere
Petroleum
Years ago, We had k500monel that had yield strengths in the 130ksi range. I am discovering that most k500 that is available is 95ksi-110ksi. Im thinking we must have had a mill run of the higher strength material where I used to work. Does anyone know if monel k500 with yield strengths around 125ksi is even available? I did find a couple of suppliers that had a 1 ft drop, but I need to find a future source. Im in search of 1.75 or 2.00" BTW.The length qty is low. The parts are only s couple of inches long, but they are very complex.
I thought that maybe I could buy it in the "annealed" condition, then heat treat it to get the numbers up. The heat treater I use said that he had a spec he could try, but he has never treated monel before. Can anyone tell me if it is very uncommon to find k500 monel round bar with yield strengths of around 125ksi? THe Nace spec states that monel be no harder than 35rC. It would be easier to machine and less likely to gall with the mating parts compared to inconel 718. Am I beating a dead horse? If it is not readily available for future use than we have to use inconel.
I thought that maybe I could buy it in the "annealed" condition, then heat treat it to get the numbers up. The heat treater I use said that he had a spec he could try, but he has never treated monel before. Can anyone tell me if it is very uncommon to find k500 monel round bar with yield strengths of around 125ksi? THe Nace spec states that monel be no harder than 35rC. It would be easier to machine and less likely to gall with the mating parts compared to inconel 718. Am I beating a dead horse? If it is not readily available for future use than we have to use inconel.