Dear All,

I need the Modulus of Elasticity for some calculation. I have some values, but I am in doubt if it can be calculated with the values. The values I have are:

Rm = 1580 MPa
Rp0.2 = 665 MPa
Elongation 55 %

These are the values of stainless steel 316L at -253°C. now I need the E-modulus. In another thread I found E=1580/0.002 but I am doubting if this is correct.

Can anyone help me in finding the right value or calculation method?

thanks in advance.

Robert
 
Replies continue below

Recommended for you

55% elongation at -253C?? Seems like you have a data problem.

The 2% offset formula you were given is for normal temperatures. Steel properties are affected by temperature, both low and high, so I doubt the formula holds for your conditions.
 
Thanks Ron,

the values I have received from the stainless steel foundation and they put the source at ASM Specialty Handbook. So I assumend the data was OK.

Do you have any data on this or know where I should try? -253C is a far more then i need and requested, but apparently the only one they had. I need approx -50C, and then the E-module and the yield strength.

Hope you, or anyone else, can tell me where I could find this information.

Robert
 
rbastiaan

The value of the elastic modulus above is valid for service temperatures below ambient for 316L stainless steel. You can use the reported yield strength (0.2% offset) for room temperature down to -50 deg C for 316L stainless steel.
 
Hi Metengr,

Thanks for your quick reply! this is what i needed. I will use your information for my further research.

thanks again.

Robert
 