Normankhan

Materials
Dec 30, 2009
15
Hi
Need your feedback on MOC.
Currently we are using FRP epoxy pipes to transfer Titanium dioxide pigment from treatment tank to other equipment. we want to shift MOC of piping from FRP to CPVC?? Can you comment on new suggested MOC.The tank mainly contain TiO2 pigment and some fraction of Sand, Al2O3, NAOH, H20. As per Bechtel piping design classifications it is recommended in using both type of Materials for transferring TiO2.
reply at earliest
Noman

 
Replies continue below

Recommended for you

I question the safety using CPVC in a manufacturing environment.
The material is simply not rugged enough to withstand normal wear & tear -- banging, struck by, walk on.
Potential pipe breakage and personnel exposure to chemicals.
 
Chance17- that's a bit of an extreme viewpoint. People still use GLASS PIPING in industrial environments and do so safely. While its use for compressed gases is definitely a concern, there is nothing intrinsically unsafe about using CPVC for LIQUID services, provided the piping is designed with the properties of this material in mind.

As to its suitability for abrasive slurry services, that's a matter of particle size, slurry % solids, temperature, pressure, expected service life etc. etc. For shorter-term projects we've had good success with it in fairly abrasive corrosive + erosive slurry services when properly designed .

Above about 4-6"NPS, CPVC becomes pretty spendy as well. In my experience FRP isn't of much use BELOW 4", and isn't available (or shouldn't be) below about 2".
 