braceh
Structural
- Jul 21, 2009
- 10
I am a CWI working under AWS D1.1 almost %100 of the time and I have a question. Is there anywhere in the code that directly prohibits the use of both SMAW E7018 and FCAW E71T-8 electrodes to compile the same weld? A contractor is proposing to tack weld with E7018 and complete final welding with E71T-8. I think the obvious solution from an inspector's stand point would be, "please show me your WPS for this," since table 4.5 item# 4 under filler metal says that a WPS written for classification A5.1 would not be applicable to a weld performed under classification A5.20 and vice-versa. However, I am asking from more of a structural and metallurgical standpoint as it might be possible to perform a WPS qualification using the two processes. Any help would be appreciated...