Is there a minimum weld size allowed when using 1/16 dia. metal cored wire?
 
Replies continue below

Recommended for you

Minimum weld size is more generally controlled by the thickness of the material being joined. If you try to put too small of a weld on a thick plate, you don't get sufficient heat input to make the weld "stick" to the underlying material.
 
Thanks for the reply ajh1. My company is trying to use 1/16 wire on 1/4" plate and that calls for a 3/16" weld bead. I was wondering if 3/16 is too small of a bead to try to get with 1/16 wire on 1/4" plate.
 
mineweld;
I would use 1/8" diameter wire for what you need to accomplish.
 
You used the term "metal cored wire" - as if this were MIG welder. True?

(Metengr: A 1/8 rod (SMAW ?) seems to be very large for a small 3/16 fillet on a 1/4 plate base metal. For a 3/16 fillet weld, most of my commercial welders prefer to use the smaller diameter (usually TIG) rods.)
 
racookpe1978;
Yes, the 1/8" diameter would be max for SMAW for this size fillet weld.
 
Sorry for the confusion, the wire I was talking about is a 1/16" dia, metal cored, tubular, GMAW wire. were using the 60# spools.
 
You'll never move fast enough to consistently produce 3/16 fillets with a 1/16 wire. Even with .045, you will likely still see oversized fillets.
 
I agree with Mr168.

You should look at the data sheet provided by your filler metal manufacturer. They will usually provide this type of information on them.
 
I'd think a an 0.035 (maybe 0.030) MIG wire would be be a good choice for a small 3/16 fillet.

But that's based on a my experience with solid wire (gas shielded) so a flux-core slighly larger diameter would probably have about the same amount of metal deposited "per sec" into the puddle.
 
The pocket-size Millermatic Calculator recommends .035" or .045" MIG wire for 1/4" thickness. It also recommends .045" or 1/16" FCAW wire for the same thickness. I would go with the smaller diameter but wire speed and voltage depends on whether you desire short circuit or spray transfer. With .035" MIG the calculator suggests 360-380, 180-190 amps, 21-22 volts, C25 shielding for short circuit or 400-420 IPM, 200-210 amps, 24-25 volts and Ar98-2%Oxygen shielding for spray.
 
For Flux-cored wire 0.045" you will have a hard time getting a welder to move fast enough for 3/16" fillet.

perhaps the GMAW would be a better choice
 