Can anyone help me in determining required minimum reinforcing in a precast slab. The slab in question is a cover for a pit. Loads are not significant. Minimum reinforcing governs the design. ACI code doesn't address this issue specifically.
 
Replies continue below

Recommended for you

Minimum ratio of reinforcement area to gross concrete area is often specified at 0.0020 for deformed bars; maximum bar spacing of 12" center to center; minimum bar size #4.
 