I've been trying to figure out what the minimum fillet weld size was changed from being based on the thickness of the thicker part joined to being based on the thickness of the thinner part joined. The commentary really only says that AWS has been doing it that way for years and AISC is just catching up. I've found a few articles that talk about the prevalence of low hydrogen electrodes, but again, nothing specific.
I sent an email to AISC regarding this a week ago and haven't gotten a response yet. Does anyone have any information on this or know of someplace I can read about it?