Dear all,
Anyone know about the minimum carbon Wt% for API 5L X60. According to the specification the maximum carbon content 0.28 wt%. My PMI results shows the carbon content of 0.05 wt%. However the microstructure is tempered martensite with the hardness of 210HV, Yield strength of 520 MPa, UTS=564 MPa and elongation is 31.5%. Mn content is 1.33 wt.%. Is the carbon content sufficient to form martensite? Is the carbon content represent hardness and UTS value?
Any comment is highly appreciated.
Thank you
Anyone know about the minimum carbon Wt% for API 5L X60. According to the specification the maximum carbon content 0.28 wt%. My PMI results shows the carbon content of 0.05 wt%. However the microstructure is tempered martensite with the hardness of 210HV, Yield strength of 520 MPa, UTS=564 MPa and elongation is 31.5%. Mn content is 1.33 wt.%. Is the carbon content sufficient to form martensite? Is the carbon content represent hardness and UTS value?