Is there a minimum base material thickness for a CJP groove weld? (or really for any weld?) Basically, I am trying to determine whether two pipe sections can be welded together if one of them has 16 gauge steel....
 
Replies continue below

Recommended for you

I am sure AWS will have your spec - but from personal experience, welding 16 ga is a bit difficult!!
 
With the appropriate equipment, the weld described can be made. We have qualified procedures (for use in a construction environment) down to .030". And one can make welds in thinner materials WITH THE RIGHT EQUIPMENT!

 
msquared48, oh, yeah, I know guys who can weld razor blades together. Looking in a mirror.

Regards,

Mike
 
msquared48

Do you mean that all of those stainless steel aircraft exhaust pipes I welded, can't be done?

B.E.

The good engineer does not need to memorize every formula; he just needs to know where he can find them when he needs them. Old professor
 
I bet all the others are only considering arc type welding, if you include electron, laser and diffusion bonding (which is solid state welding) you could join almost anything.
 
You need the proper equipment and properly trained people for any task.

Al

Best regards - Al
 