Coating requirment please explain how this materail is applied and to what extent does it affect the dimensional requirements of machined part after application. Is it necessary to make allowance for coating?
 
Replies continue below

Recommended for you

KHI...

RE: MIL-M-3171 [now: AMS-M-3171] coating... which "Type"???

Regards, Wil Taylor
 
The coating is applied as a Type VI
 
KHI...

REF Ty VI: as with most chem films, there is virtually NO measureable thickness +/- change. There will probably be an increased thickness of +0.0001-inch (+0.0025-mm)... if it could be measured (I doubt if conventional measurement instruments would see any difference).

Regards, Wil Taylor
 