Hi all
Recently, we got a serious hinge and base broken issues and we sent defect samples to SGS lab. for MFI analysis, data shows MFI change from 22(raw material) to 28 g/10min under ASTM D-1238 260degree/2.16kg, We doublt that large ratio of re-cycle material has been added during the process.
Any idea ? or suggestion.
Tks