I have a formed channel 1.25 legs x 2.2 height 19" long, 0.25" thickness, A36 material, with an inside bend radius of 0.18". The channel is loaded with a 1.5" dia roller that rides against the legs of the section. The loading is not extreme, usually around 500 lbs. We see the channel opening up, on the loaded side, by an average of 0.030" after 20,000 cycles. We would like there to be zero deformation and are considering a bend radius of 0.25 to help the situation.
I am concerned that the tight bend radius is causing this issue. Will increasing the bend radius provide a solution entirely or will thermal stress relief have to be added as a post op.?
Allied Systems Company
- Long Reach Attachments
I am concerned that the tight bend radius is causing this issue. Will increasing the bend radius provide a solution entirely or will thermal stress relief have to be added as a post op.?
Allied Systems Company
- Long Reach Attachments