I am considering a change from water-based cutting fluid to oil (mineral or vegatable) on 13 Acme Gridley 8-spindle bar machines. The material we are running is 1215 with the traditional tooling and speeds for these machines. We are considering this for better lubrication of both the cutting tools and machine.
There are many issues to consider (i have 5 pages of them). Does any one have experience in going back to oil after using water based fluids for bar turning.