Good afternoon,
Please share your experiences regarding MEG reclamation units corrosion, particularly in the circuits handling MEG solution saturated with salts. Only found one paper about this (NACE 07116). Licensor is specifying all these circuits (downstream of Sour gas Stripper) in carbon steel (with 6mm CA). This includes reclaimer bottom (hot) loop and associated downstream piping and equipment.
I honestly have some concerns related with O2 ingress and with salt deposits accumulation, which may cause Carbon Steel to corrode and experience pitting.
I would appreciate if you can share your experience. Normal operating conditions are pointed below.
Solution: 90%wt MEG + 10%H2O saturated with NaCl salts.
H2S and CO2 is pointed to be 0%mol, assuming all was previous stripped in the upstream Sour Gas Stripper (through N2 injection) and on the Vacuum Reclaimer.
Temp.= 150 F to 250 F (reclaimer bottom loop)
Kind regards,
Please share your experiences regarding MEG reclamation units corrosion, particularly in the circuits handling MEG solution saturated with salts. Only found one paper about this (NACE 07116). Licensor is specifying all these circuits (downstream of Sour gas Stripper) in carbon steel (with 6mm CA). This includes reclaimer bottom (hot) loop and associated downstream piping and equipment.
I honestly have some concerns related with O2 ingress and with salt deposits accumulation, which may cause Carbon Steel to corrode and experience pitting.
I would appreciate if you can share your experience. Normal operating conditions are pointed below.
Solution: 90%wt MEG + 10%H2O saturated with NaCl salts.
H2S and CO2 is pointed to be 0%mol, assuming all was previous stripped in the upstream Sour Gas Stripper (through N2 injection) and on the Vacuum Reclaimer.
Temp.= 150 F to 250 F (reclaimer bottom loop)
Kind regards,