Will Mobil 1 Synthetic based barrier fluids attack mechanical seals with Carbon vs. Tungsten Carbide faces?
 
Replies continue below

Recommended for you

No it will not attack it however be sure you have the right grade of carbon because you may experience Blistering. This occurs when the oil is absorbed by the carbon and when the seal runs it generates heat. The oil inside the carbon expands and little blisters occur as the oil expands damaging the carbon.

trust this helps.
 
In my experience blistering happens more often with heavier viscosities, ISO 32 and above. Mobil Synturon 6, if I remember correctly, is around 22, and should not be a problem.
 
Blistering is not caused by absorption into the carbon material; it is a byproduct of viscous shear. Therefore, ANY carbon will blister provided the prime conditions exist. Prime conditions for blistering include higher seal face pressures and speeds, higher viscosity fluids, and frequent stop/start cycling (constant speed should not result in blister formation).

All that being said, if you use a premium grade of carbon (metal filled as opposed to a resin-filled) you reduce your chances of this occurring. The resin impregnated carbon face surface smoothness may also promote blister formation. Based on experience, you should be fine with the Synturion 6, but I would verify the carbon grade you have installed to be sure.
 