Jul 18, 2007 #1 salobrena Aerospace Joined Nov 10, 2005 Messages 2 Location CH Can someone give me the mechanical properties and reference for SS304 1/4 Hard Tubing per MIL-T-5695. MMPDS has the properties for plate but not for tubing. Thank you in advance.
Can someone give me the mechanical properties and reference for SS304 1/4 Hard Tubing per MIL-T-5695. MMPDS has the properties for plate but not for tubing. Thank you in advance.
Jul 18, 2007 1 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US You can view the document yourself here: http://assist.daps.dla.mil/quicksearch/ Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
You can view the document yourself here: http://assist.daps.dla.mil/quicksearch/ Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Jul 18, 2007 #3 YoungTurk Mechanical Joined Jul 16, 2004 Messages 333 Location US Great link, definitely getting bookmarked! Upvote 0 Downvote
Jul 18, 2007 Thread starter #4 salobrena Aerospace Joined Nov 10, 2005 Messages 2 Location CH Thank you for the link, however, the only way to get the information is to subscribe and pay for the document. Am I correct or not? Upvote 0 Downvote
Thank you for the link, however, the only way to get the information is to subscribe and pay for the document. Am I correct or not?
Jul 18, 2007 #5 rb1957 Aerospace Joined Apr 15, 2005 Messages 16,139 Location CA nope ... search for 5695, it'll return a hit, click on it, scroll down, click on rev D, opens up without charging you anything Upvote 0 Downvote
nope ... search for 5695, it'll return a hit, click on it, scroll down, click on rev D, opens up without charging you anything